Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7115 - Americas - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7115 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
NORYL PPX™ 7115 resin is a non-reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade exhibits high modulus, high-temperature performance, excellent melt strength, impact resistance, hydrolytic and dimensional stability. NORYL PPX7115 resin is an excellent candidate for applications requiring high modulus and chemical resistance.

UL Yellow Card Link E121562-221243
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 12 cm³/10min ISO 1133
Temperatura 260 °C -
Carga 5 kg -
ASTM Data
Índice de fluidez, MFI 14 g/10min ASTM D 1238
Temperatura 260 °C -
Carga 5 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1370 MPa ISO 527
Esfuerzo de fluencia 35 MPa ISO 527
Alargamiento a rotura 50 % ISO 527
ASTM Data
Módulo de tracción 1240 MPa ASTM D 638
Esfuerzo de fluencia a tracción 35 MPa ASTM D 638
Esfuerzo de fractura a tracción 34 MPa ASTM D 638
Alargamiento a la fluencia 8 % ASTM D 638
Alargamiento a la rotura 125 % ASTM D 638
Módulo de flexión 1370 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 534 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. reblandecimiento Vicat, A 131 °C ISO 306
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
ASTM Data
Estabilidad al calor @ 66 psi 112 °C ASTM D 648
Estabilidad al calor @ 264 psi 85 °C ASTM D 648
Temperatura Vicat 86 °C ASTM D 1525
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 990 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 60 - 65 °C -
Tiempo de pre-secado 2 - 4 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 260 - 290 °C -
Temperatura del molde 30 - 50 °C -
Zona 1 225 - 275 °C -
Zona 2 240 - 280 °C -
Zona 3 250 - 290 °C -
Velocidad de giro de husillo 20 - 100 rpm -
Contrapresión 0.3 - 0.7 MPa -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Disponibilidad regional
Norteamérica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.